1 October 1990 Preparation of La1-xSrxCoO3 (x=0,0.3) by two solution routes
H. Kido, Sridhar Komarneni
Author Affiliations +
Abstract
La i xSrxCoO3 (0, 0.3) were prepared by two solution methods using water and hexanoic acid as solvents, respectively. The single phase of LaCoO3 was obtained at 600CC the case of hexanoic acid route, which was about 300'C lower than in the other case with water alone. It was possible to make thin films of the perovskite compounds by controlling the viscosity of the hexanoic acid solutions. These perovskite materials are expected to have applications as oxidizing catalysts in automobiles, as electrodes for zirconia heaters and as cathode materials for C02 lasers.
© (1990) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
H. Kido and Sridhar Komarneni "Preparation of La1-xSrxCoO3 (x=0,0.3) by two solution routes", Proc. SPIE 1307, Electro-Optical Materials for Switches, Coatings, Sensor Optics, and Detectors, (1 October 1990); https://doi.org/10.1117/12.21659
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
X-ray diffraction

Metals

Electro optical sensors

Perovskite

Sensors

Thin film coatings

Optical coatings

Back to Top