Abstract
Welding is one of the very common process in industrial production. It is a kind of manufacturing process and technology which joint mental or other thermoplastic materials by heating, high temperature or high pressure. Welding quality will directly affect the final quality of workpiece. So during the welding process, each links have strict standard and welding quality evaluation has different indicators. Therefore, how to make a rapid detection to weld defect has become a valuable research. This topic is aimed at weld defect detection of small workpiece. The study contains the selection of sensor, design of detection system, hardware platform, software design, user interface design, etc. In the end, a set of high accuracy detector of weld defect will be designed.
© (2016) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Kelin Hu and Chao Gao "The research of weld defect detection based on high precision displacement sensor", Proc. SPIE 10023, Optical Metrology and Inspection for Industrial Applications IV, 1002325 (24 November 2016); https://doi.org/10.1117/12.2247889
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Sensors

Defect detection

Servomechanisms

3D modeling

Nondestructive evaluation

Image processing

3D image processing

Back to Top