27 March 2022 Effects of multi-pulses on material removal threshold of superalloy irradiated by ultra-short pulsed lasers
Author Affiliations +
Proceedings Volume 12169, Eighth Symposium on Novel Photoelectronic Detection Technology and Applications; 121699N (2022) https://doi.org/10.1117/12.2625457
Event: Eighth Symposium on Novel Photoelectronic Detection Technology and Applications, 2021, Kunming, China
Abstract
The effects of femtosecond laser (wavelength 1035nm, pulse duration 400 fs, pulse repetition rate 1kHz) on the material removal threshold of superalloy was experimentally investigated, specifically the influence of pulse number irradiated on the threshold of superalloy. Irregular bulge structures were found at the bottom of ablation holes. Two sets of material removal thresholds are derived from the value of hole diameter and depth, which are 0.506 J/cm2 , 0.245 J/cm2 , 0.124 J/cm2 , 0.102 J/cm2 , 0.096 J/cm2 and 0.141 J/cm2 , 0.130 J/cm2 , 0.031 J/cm2 , 0.026 J/cm2 , 0.091 J/cm2 for diameter derivation and depth derivation, respectively, for 1, 10, 100, 500 and 1000 pulses. The deduced two sets of thresholds show similar behavior that the threshold sharply decreases with the pulse number and levels out as the pulse number exceeds 100. The phenomenon is due to incubation effects of multi-pulse irradiation on the surface of superalloy and the incubation coefficient for the thresholds calculated by diameter and depth is fitted to be ~0.72 and ~0.77.
© (2022) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Yun Gao, Ze-nan Yang, Cheng-wei Song, Yuan-hang Zhang, Jian Zhang, Qing-hua Zhang, Min-cai Liu, and Ya-guo Li "Effects of multi-pulses on material removal threshold of superalloy irradiated by ultra-short pulsed lasers", Proc. SPIE 12169, Eighth Symposium on Novel Photoelectronic Detection Technology and Applications, 121699N (27 March 2022); https://doi.org/10.1117/12.2625457
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Laser ablation

Laser damage threshold

Femtosecond phenomena

Pulsed laser operation

Ultrafast lasers

Metals

Applied physics

Back to Top