16 February 2004 High-temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers
Author Affiliations +
Proceedings Volume 5648, Smart Materials III; (2004) https://doi.org/10.1117/12.580720
Event: Smart Materials, Nano-, and Micro-Smart Systems, 2004, Sydney, Australia
Abstract
Al2O3 reinforced by SiC whiskers (Al2O3/SiC-W) was sintered in order to investigate the fatigue strength of crack-healed specimens at high temperature. A semi-elliptical surface crack of 100μm in surface length was introduced on each specimen surface. These specimens were crack-healed at 1300°C for 1 h in air, and static and cyclic fatigue strengths were systematically investigated at room temperature, 900°C, and 1100°C by three-point bending. The static and cyclic fatigue limits of the crack-healed specimens were more than 70% of the average bending strength at each testing temperature. Crack-healed specimens of Al2O3/SiC-W were not sensitive to static and cyclic fatigues at room temperature and high temperatures. Therefore, the combination of crack-healing and whisker reinforcement can play an important role in increasing static and cyclic fatigue strengths at high temperature.
© (2004) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Kotoji Ando, Sang-Kee Lee, Koji Takahashi, and Masahiro Yokouchi "High-temperature fatigue strength of crack-healed Al2O3 toughened by SiC whiskers", Proc. SPIE 5648, Smart Materials III, (16 February 2004); https://doi.org/10.1117/12.580720
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Aluminum

Silicon carbide

Ceramics

Scanning electron microscopy

Failure analysis

Particles

Photomicroscopy

Back to Top